Galvanic corrosion can happen when dissimilar metals, stainless steel and aluminum, for example, are in contact with each other, exposed to an electrolyte, and an electrical current is applied. That’s the technical definition. The layman’s definition is it’s the white stuff that grows around your stainless steel fasteners in your aluminum mast and boom when…